Place of Origin: | CHINA |
Brand Name: | LiangRu |
Certification: | ISO9001 |
Model Number: | LR |
Minimum Order Quantity: | Different goods has different MOQ |
---|---|
Price: | Different goods has different price |
Packaging Details: | As per customer¡¯s requirement or our usual packaging way |
Delivery Time: | 10-15days |
Payment Terms: | T/T,L/C or others |
Supply Ability: | sufficient supply |
Palce Of Origin: | CHINA | Fuction: | Engrave |
---|---|---|---|
Application: | Textile Rotary Printing | Name: | Photo Emulsion |
Condition: | New | Brand Name: | LR |
Laser Photo Emulsion For Rotary Printing Screens In Chemical
Milky white emulsion for laser stencil making.
High sharpness of separation, convenient process and fine accuracy.
Suitable for squeegee or magnetic rotary screen printing machine.
Laser engraving:
Make the stencil by laser generator after color separation by computer in according with patterns.
Package:
5kg per plastic barrel, and 20kg per export carton.
Storage:
One year at 5-35¡æ(in a dark and dry place).
Application:
1.Washing the screen:
Immerse the screen into Cleaning liquor for nickel screen for around 10 minutes, take out and rinse with water, then dried at low temperature in an oven. At the same time, prevent the screen from being stained with dirt(It is necessary to wear protective gloves avoiding corrosiveness).
2.Preparing the photosensitive emulsion:
It should be operated under a gentle yellow light(prohibit from operating in no opacifying condition).35-50ml of photosensitizer solution is added into 1000g of photoemulsion, stir clockwise until to homogenous, stand for 1-2 hours to let off bubbles in a cool and dark place. Then maintain the prepared photoemulsion at 5-15¡æ in a constant temperature storage box (a seal cover is needed to avoid skinning).
3.Coating:
300g of the prepared emulsion is added into a clean scraper ring and coated on the clean screen with a speed of 10-12cm/min, then dried at 35-40¡æ and 60% relative humidity in an oven with circle wind and no more than ¡À2¡æ temperature differences.
4. Exposure:
Fixed the coated screen on an exposure machine and fit the manuscript closely
The fit time should be determined after trial. Reference time: 5-8 times on a scanning machine or 1-3 minutes on a stationary exposure machine.
5. Developement:
The exposed screen should develop timely by putting it in water at 5-30 for approx. 3-5 minutes, then washed until patterns appear clearly, then rinse off the leaked emulsion with water under low pressure, and dried at 50-60 in a constant temperature oven.
6. Curing:
Curing the retouched screen at 180 for 2 hours in a constant temprature oven until the film becomes golden, then take out to bind with endring after cooling down.
Black Roll Cotton Stenter Brushes Wheel Mini For Textile Machinery
Custom Textile Machinery Spare Parts Color Paste Pump For Rotary Screen Printing
Stainless Steel Expanding Roller Opener Cylinder Hydraulic High Stability
Textile Machinery Flat Selvedge Uncurler Electrical For Stenter Nylon
High Strength Guided Vertical Clip Chain Smooth For Stenter Machine Patrs
Manganese Stenter Machine Parts Anti - Rust Germany Krantz Pin Holder
High Density Rotary Printing Machine Spares , 20mm Rotary Magnetic Rod
Elastic Rotary Printing Machine Spares Dimensional Stability Aluminum 640 End Rings
640 Die Cast Rotary Printing Machine Spares Zimmer Type End Ring